To reduce early-age shrinkage plastic cracking in hot, windy desert site conditions, the best on-site action is which?

Choices

  • (A) Continuous moist curing of exposed surfaces (evaporation control)
  • (B) Postpone 28-day testing only
  • (C) Increase w/cm regardless
  • (D) Skip finishing to save time

Correct answer: (A)

Continuous moist curing of exposed surfaces (evaporation control)

Explanation

ACI 305/302 heat guidance: limit evaporation rate (curing, wind screens).